The influence of roller burnishing process parameters on surface quality and fatigue life of AA 7075-T6 alloyEinfluss der Parameter des Rollierprozesses auf die Oberflachenqualitat und die Ermudungslebensdauer der Aluminiumlegierung EN AW-AlZn5,5MgCu-T6

dc.authorscopusid57210143311
dc.authorscopusid6505647210
dc.authorscopusid57671328800
dc.authorwosidÇelik, Mahmut/AAL-7669-2021
dc.contributor.authorÇelik, Mahmut
dc.contributor.authorÇaydaş, Ulaş
dc.contributor.authorAkyuz, M.
dc.date.accessioned2022-09-04T10:27:00Z
dc.date.available2022-09-04T10:27:00Z
dc.date.issued2022
dc.departmentFakülteler, Mühendislik-Mimarlık Fakültesi, Makine Mühendisliği Bölümüen_US
dc.departmentFakülteler, Mühendislik-Mimarlık Fakültesi, Makine Mühendisliği Bölümüen_US
dc.description.abstractRoller burnishing method is a low-cost and effective surface treatment method that has been frequently preferred in recent years. In this method the surface roughness is minimized by small plastic deformations, without removing chips from the surfaces, caused by the rolling element pressed against the surface with a certain force. While the surface hardness of the material increases in the process, the surface roughness decreases significantly. In this study, the effects of the process parameters of roller burnishing method (burnishing pressure and number of passes) on AA7075-T6 aluminum alloy in terms of fatigue strength and surface roughness were investigated experimentally. Taguchi L9 experimental design method was used in the study, and the burnishing process was carried out by a specially produced disc-shaped apparatus. As a result of the study, it was determined that the roller burnishing method increased both the fatigue strength and surface quality of AA 7075 T6 alloy. In consequence of roller burnishing, it was determined that fatigue life and surface roughness values improved by 116 % and 96 %, respectively.en_US
dc.description.sponsorshipFirat University Projects of Scientific Investigation Unit [TEKF.18.07]en_US
dc.description.sponsorshipThis work was supported by Firat University Projects of Scientific Investigation Unit. (Project number: TEKF.18.07).en_US
dc.identifier.doi10.1002/mawe.202100291
dc.identifier.endpage616en_US
dc.identifier.issn0933-5137
dc.identifier.issn1521-4052
dc.identifier.issue5en_US
dc.identifier.scopus2-s2.0-85129651327
dc.identifier.scopusqualityQ3
dc.identifier.startpage608en_US
dc.identifier.urihttps://doi.org/10.1002/mawe.202100291
dc.identifier.urihttps://hdl.handle.net/20.500.12639/4687
dc.identifier.volume53en_US
dc.identifier.wosWOS:000790869500008
dc.identifier.wosqualityQ4
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.institutionauthorÇaydaş, Ulaş
dc.language.isoen
dc.publisherWiley-V C H Verlag Gmbhen_US
dc.relation.ispartofMaterialwissenschaft Und Werkstofftechniken_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectRoller burnishing; surface treatment; fatigue strength; AA 7075-T6; surface qualityen_US
dc.subjectMagnesium Alloy; Ball; Roughness; Performance; Hardness; Enhancement; Roundness; Strength; Finishen_US
dc.titleThe influence of roller burnishing process parameters on surface quality and fatigue life of AA 7075-T6 alloyEinfluss der Parameter des Rollierprozesses auf die Oberflachenqualitat und die Ermudungslebensdauer der Aluminiumlegierung EN AW-AlZn5,5MgCu-T6en_US
dc.title.alternativeEinfluss der Parameter des Rollierprozesses auf die Oberflächenqualität und die Ermüdungslebensdauer der Aluminiumlegierung EN AW-AlZn5,5MgCu-T6en_US